`Revolve N-525 (6056) Natural (appears white coloured) & BH3239 Black (black coloured)`. Polyethylene materials manufactured by rotational moulding. For use with water up to 85°C.
'XYRON WG732 AWY2266, WG732 AWY2269, WG732 AWY6628, WG722 AWY6627, W5002 AWY1208, W5002 AWY2267, W5002 AWY6629, W5002 AWY3326, WG722 AWY2261, WG732 AWY3325, WG722 AWY3324 & WG733 ABY3315'. Injection moulded, black, grey or beige coloured PPE materials manufactured in Thailand & China. For use with water up to 85°C.
‘Tecomid HT NT40 GR30 BK009 01 QW, Tecomid HT NT40 GR35 BK009 01 QW, Tecomid HT NT40 GR40 BK009 01 QW, Tecomid HT NT40 GR45 BK009 01 QW, Tecomid HT NT40 GR50 BK009 01 QW, Tecomid HT NT40 GR55 BK009 01 QW & Tecomid HT NT40 GR60 BK009 01 QW’. Black coloured, injection moulded glass-fibre reinforced PPA materials. For use with water up to 85°C.
'USW-95-A Black'. Black coloured, injection moulded TPU material. For use with water up to 23°C.
`Superfast Copper`. Site applied, copper coloured epoxy putty. The putty should be kneaded together, its supplied in a pre-measured 1:1 mass ratio and applied as per manufacturer's directions for use dated August 9th, 2021. Cure for 24 hours@22°C. For use with water up to 23°C. This material is only approved for the curing conditions that appear on the approval. If the cure conditions are varied from those specified on the approval then the material is not covered by the scope of the approval.
Page 111 of 802
We use cookies to give you the best possible experience with WRAS. Some are essential to provide website functions and ensure the website is secure. We also use cookies to help us understand how people use the site and to make improvements. Click "Accept All" to enable recommended settings or click "Manage cookies" to adjust your settings. For more details, see our Cookie Policy.