Section Code 5265 : Material only. Components made from materials listed in this section may require to be submitted for audit tests.
Back To Directory Sections'Tatren HG 10 07'. White coloured, injection moulded polypropylene material. For use with water up to 85°C.
'Sabic 576S'. White coloured, injection moulded polypropylene material. For use with water up to 85°C.
'BA160E-8229-01'. Black coloured, injection moulded polypropylene material. For use with water up to 85°C.
'Verplen C3008 VE ACLKUV W (GF 30% green coloured) & Verplen 60NE A W (black coloured'. Injection moulded, polypropylene materials. For use with water up to 60°C.
'Borealis HE125MO & Bn HE125MO-100'. White coloured (semi-opaque), injection moulded PP-H materials. For use with water up to 85°C.
'CoolPro Tan/Black'. Extruded, reinforced polypropylene sheet which is beige coloured on one side (water contact side) and black coloured on the other (non-water contact side). For use with water up to 23°C.
'Hostalen PP H4122 103220'. Polypropylene material for injection moulding and compression moulding. For use with water up to 23°C.
'RA7050-GN (Green), RA7050-LG (Light grey) & RA7050 (Grey)'. PP-RCT materials for injection moulding and extrusion purposes. For use with water up to 85°C.
Page 2 of 2
We use cookies to give you the best possible experience with WRAS. Some are essential to provide website functions and ensure the website is secure. We also use cookies to help us understand how people use the site and to make improvements. Click "Accept All" to enable recommended settings or click "Manage cookies" to adjust your settings. For more details, see our Cookie Policy.